3M DP420LH

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M DP420LH

Main features

  • 2:1 Epoxy Mixing by Volume
  • 20-Minute Open Time
  • Low-Halogen Toughened Epoxy

Product Description

3M Scotch-Weld Epoxy Adhesive DP420LH is a low-halogen, toughened two-part epoxy adhesive for structural bonding with peel and shear strength and resistance to impact and fatigue. Base and accelerator mix 2:1 by volume or 2:0.97 by weight. Typical open time is 20 minutes, while work life at 23 deg C depends on mixed mass: 30 minutes for 5 g, 20 minutes for 10 g, and 15 minutes for 20 g. The cured adhesive has typical Shore D hardness 85 at 23 deg C by ASTM D2240 and total halogen content of less than 800 ppm.

Key features

  • 2:1 volumetric mixing: The base-to-accelerator ratio is 2:1 by volume or 2:0.97 by weight.
  • Mass-dependent work life: At 23 deg C, typical work life is 30 minutes for 5 g, 20 minutes for 10 g, and 15 minutes for 20 g.
  • Low-halogen formulation: Typical cured-material values are 720 ppm chlorine, less than 5 ppm bromine, and less than 800 ppm total halogens.

Applications

Structural bonding where impact and fatigue resistance are selection factors; replacement of mechanical fastening in supported designs.

Technical Specifications

General Properties
AppearanceAppearance
Off-White
Component SystemComponent System
Two (Accelerator | Base)
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers