LOCTITE ABLESTIK 550K

Main features

  • Low cure temperature
  • Hard to bond metals
  • Thermally conductive

Product Description

LOCTITE ABLESTIK 550K is a white epoxy film designed for substrate attach and heat sink bonding. It offers high thermal conductivity and low cure temperature and comes on a glass fabric carrier.

LOCTITE ABLESTIK 550K is a non-electrically conductive, epoxy assembly film commonly used on Gold and gold plated surfaces and is suitable for an array of difficult-to-bond metals.

Cure Schedule

  • 30min @150°C
  • 2 hours @ 125°C
Product Family

ABLESTIK 550K

1. Select Package Type
2. Select Thickness
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 31 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
4392 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
102 °C
Thermal ConductivityThermal Conductivity
0.8 W/m.K
Weight Loss @ 300°CWeight Loss @ 300°C
0.37 %
Electrical Properties
Volume ResistivityVolume Resistivity
7200000000000 Ohms⋅cm

Additional Information

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers