BOSTIK HM7116

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

BOSTIK HM7116-98

Main features

  • Moderate Open-Time Hot-Melt Processing
  • Plasticizer-Migration Resistance for Vinyl
  • Good High-Temperature Resistance

Product Description

Bostik HM7116 combines moderate open time, low application viscosity, and good high-temperature resistance in a polyester hot melt adhesive for wood, textiles, vinyl film, and related product-assembly substrates. The light amber granular material is typically applied at 400 to 450 deg F using slot-die, spray, or hot-melt gravure equipment. Resistance to plasticizer migration is relevant for vinyl-film constructions, while a 125 deg C SAFT result characterizes elevated-temperature adhesive performance. Edgefold and general product assembly are established uses for this polyester hot-melt grade.

Key features

  • Moderate open time: Provides a medium relative open time at 200 deg C for hot-melt assembly.
  • Low application viscosity: Melt viscosity is 28,000 cP at 215 deg C for hot-melt application.
  • Plasticizer migration resistance: Resists plasticizer migration in vinyl-film bonding applications.

Applications

Bonding textiles, vinyl films, wood, edgefold constructions, and general product-assembly substrates.

Product Family

BOSTIK HM7116

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Light amber granules
Density (g)Density (g)
1.25 g/cm3
Physical Properties
ViscosityViscosity
28000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceLight amber granulesAs supplied
Softening point137deg CB&R softening point
Melt point127deg CDSC
Melt viscosity28,000cP215 deg C
Density1.25g/ccTypical physical property
Relative open timeMedium200 deg C
Shelf life1year23 deg C; sealed containers
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile strength3,940psi25 deg C; typical physical property
Elongation500%25 deg C; typical physical property
SAFT125deg C1000 g/in^2 load; 5 deg C/min

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF