ECCOBOND 334-1

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ECCOBOND 334-1

Main features

  • 8-Hour Work Life at 25 deg C
  • Moisture Cure in About 1 to 4 Days
  • One-Part Tungsten-Filled RTV

Product Description

LOCTITE ECCOBOND 334-1 is a one-part, gray tungsten-filled RTV silicone sealant for room-temperature moisture cure. The material is applied without component mixing and has a typical work life of 8 hours at 25 deg C. Cure typically takes about 1 to 4 days at 25 deg C, depending on relative humidity and bond width. Henkel does not recommend bond lines greater than 1 inch wide because moisture cannot readily reach the center of wider sections. After cure, the material forms a relatively flexible silicone seal for applications where a flexible RTV material is specified.

Key features

  • 8-Hour Work Life at 25 deg C: Typical work-life value applies to the one-part RTV silicone before cure.
  • About 1 to 4-Day Moisture Cure: The listed cure range applies at 25 deg C.
  • Tungsten-Filled RTV Silicone: The gray one-part formulation cures to a flexible material without component mixing.
Product Family

ECCOBOND 334-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Gray
Work life @25°CWork life @25°C
8 hours

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Work life8h25 deg C; typical
Storage life122days25 deg C; continuously dry; typical
Cure schedule1 to 4days25 deg C; depends on relative humidity and bond width

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers