LOCTITE 3872

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 3872

Main features

  • Self-Shimming Thermal Bondline
  • UV Fixture Before Heat Cure
  • Low-Modulus Thermal Attachment

Product Description

LOCTITE 3872 combines a one-part acrylic-urethane adhesive with glass-sphere bondline control for thermal attachment of heat-generating devices. Solid spheres establish a 0.127 mm bondline, and UV fillet curing provides rapid fixturing before the required heat-cure step. The cured material has a typical thermal conductivity of 1.20 W/(m K), a glass transition temperature of -33 deg C, and Shore D 71 hardness after the stated cure. Its operating-temperature range is -54 to 150 deg C. Applications include bonding power devices to heat sinks, including silicon chips to metal lead frames.

Key features

  • Self-Shimming Bondline: Solid glass spheres establish a uniform 0.127 mm bondline.
  • Thermal Bond Performance: Typical cured thermal conductivity is 1.20 W/(m K).
  • UV Fixture Before Heat Cure: UV fillet cure fixtures parts before the full heat-cure step.

Applications

Applications include bonding heat-generating devices to heat sinks, including silicon chips to metal lead frames.

Product Family

LOCTITE 3872

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

General Properties
AppearanceAppearance
Light grey, thick dispersion
Specific GravitySpecific Gravity
2.50
Physical Properties
ViscosityViscosity
550,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
-33 °C
Operating TemperatureOperating Temperature
-54 to 150 °C
Thermal ConductivityThermal Conductivity
1.20 W/m.K
Mechanical Properties
ElongationElongation
30 %
Electrical Properties
Dielectric StrengthDielectric Strength
9.84 kV/mm
Volume ResistivityVolume Resistivity
2.4×10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-Supplied Properties

PropertyValueUnitMethod / condition
AppearanceLight grey, thick dispersion-Uncured
Specific gravity2.50-25 deg C
Viscosity1,200,000 to 2,100,000mPa sBrookfield HBT, spindle TB, 0.5 rpm, helipath, 25 deg C
Viscosity550,000mPa sBrookfield HBT, spindle TB, 5.0 rpm, helipath, 25 deg C
Spacer sphere diameter0.127mmSolid glass spheres
Technical properties

Final-State Properties

PropertyValueUnitMethod / condition
Thermal conductivity1.20W/(m K)ASTM E 1225; cured 45 min at 125 deg C
Hardness71Shore D-2ASTM D 2240; cured 45 min at 125 deg C
Tensile strength at break3.70N/mm^2Cured 45 min at 125 deg C
Elongation at break30%Cured 45 min at 125 deg C
Young's modulus117N/mm^2Cured 45 min at 125 deg C
Glass transition temperature-33deg CCured 45 min at 125 deg C
Dielectric strength23.62kV/mmASTM D 149; cured 45 min at 125 deg C
Operating temperature-54 to 150deg CProduct operating range

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers