LOCTITE AA 312
Harmonization Code : 3506.10.5000 | HTS - Other Products Suitable For Use As Glues, Put Up For Retail Sale As Glues, Not Exceeding A Net Weight Of 1 Kg

Main features
- One-Component Formulation
- Room-Temperature Cure
- Dissimilar Material Bonding
Product Description
LOCTITE® AA 312™ is a one-component modified acrylic ester adhesive formulated for bonding dissimilar materials, including metals, glass, and ceramics. Used with LOCTITE® Activator 736™ or 734™, the adhesive cures at room temperature and provides rapid fixture times for close-fitting assemblies. Its medium-viscosity formulation requires no mixing, making it suitable for manufacturing and industrial bonding applications where fast processing and reliable bond development are required.
Key features
- One-component formulation: Requires no mixing, simplifying application and assembly processes.
- Room-temperature cure: Cures with LOCTITE® Activator 736™ or 734™ to support rapid fixture times.
- Dissimilar material bonding: Suitable for bonding metals, glass, and ceramics in close-fitting assemblies.
Applications / Suitable for
- Metal-to-metal bonding
- Glass bonding applications
- Ceramic assembly applications
- Industrial manufacturing and assembly operations
- Close-fitting bonded joints requiring fast fixturing
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Typical properties of LOCTITE® AA 312™ before curing and assembly.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Type | Modified acrylic ester | - | As supplied |
| Appearance | Clear amber liquid | - | Uncured material |
| Specific Gravity | 1.1 | - | 25°C |
| Viscosity | 850-1,200 | mPa·s (cP) | Brookfield RVT, Spindle 2, 20 rpm, 25°C |
After-processing / final-state properties
Typical cured-material properties and lap shear strength performance data.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Coefficient of Thermal Expansion | 100 × 10⁻⁶ | K⁻¹ | ISO 11359-2 |
| Thermal Conductivity | 0.1 | W/(m·K) | ISO 8302 |
| Specific Heat | 0.3 | kJ/(kg·K) | Cured material |
| Lap Shear Strength | ≥17.2 | N/mm² | ISO 4587, steel (grit blasted), 24 h @ 22°C, Activator 736™ or 734™ on 2 sides |