LOCTITE AA 3462

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE AA3462

Main features

  • Rapid UV/Visible Light Cure
  • Flexible Shock-Absorbing Bondline
  • Glass Bonding Across Multiple Materials

Product Description

LOCTITE AA 3462 is a one-part modified acrylic adhesive for UV- or visible-light-cured bonding, potting and sealing of glass-based assemblies. The translucent liquid has a typical viscosity of 9,500 to 14,300 mPa s at 25 deg C and can reach fixture in 3 seconds or less on glass under 365 nm exposure at 100 mW/cm^2 using an electrodeless D bulb. The cured material is flexible, with elongation above 150% after 30 seconds per side at 100 mW/cm^2 and 365 nm using an electrodeless D bulb, followed by 24 hours at 22 deg C. Applications include glass-to-steel, aluminum, PVC, ABS and polycarbonate assemblies. The adhesive combines rapid light cure with flexibility in these glass-based assemblies.

Key features

  • Rapid Light Fixture: Fixture can be reached in 3 seconds or less on glass at 100 mW/cm^2 measured at 365 nm using an electrodeless D bulb.
  • Flexible Cured Material: Elongation at break is above 150% by ISO 527-3 after 30 seconds per side at 100 mW/cm^2 and 365 nm using an electrodeless D bulb, followed by 24 hours at 22 deg C.
  • Glass Bonding Across Multiple Materials: Applications include glass bonded to steel, aluminum, PVC, ABS and polycarbonate.

Applications

Glass bonding, potting and sealing, including glass-to-steel, aluminum, PVC, ABS and polycarbonate assemblies.

Product Family

LOCTITE AA 3462

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Translucent, colorless to light yellow liquid
Chemistry TypeChemistry Type
Modified acrylic
Refractive indexRefractive index
1.48
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
9,500 to 14,300 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
57 °C
Mechanical Properties
ElongationElongation
>150 %
Chemical Properties
Water AbsorptionWater Absorption
2.12 %
Other Properties
Storage TemperatureStorage Temperature
2 °C to 8 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Specific gravity1.1Typical at 25 deg C
Refractive index1.48Typical uncured
Viscosity9,500 to 14,300mPa sCone and plate; shear rate 20 s^-1; 25 deg C
Depth of cureAbove 1.6mm300 mW/cm^2; measured 320 to 400 nm; 15 s; electrodeless D bulb
Fixture time3 maxsGlass; 100 mW/cm^2 measured at 365 nm; electrodeless D bulb
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Glass transition temperature57deg CISO 11357-2; cured 100 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C
Shore hardnessMinimum 80Shore AISO 868; cured 100 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C
Elongation at breakAbove 150%ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C
Tensile strength at break14.9N/mm^2ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C
Tensile modulus102.4N/mm^2ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C
Block shear, abraded steel to glass5.6N/mm^2ISO 13445; 300 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C
Block shear, aluminum to glass5.3N/mm^2ISO 13445; 300 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C
Block shear, polycarbonate to glass4.5N/mm^2ISO 13445; 300 mW/cm^2 at 365 nm for 30 s per side plus 24 h at 22 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers