LOCTITE AA 3953

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE AA 3953

Main features

  • Medium-Viscosity Flexible Bonding
  • Fast 405 nm LED Fixture
  • Flexible 233% Elongation

Product Description

LOCTITE AA 3953 is a one-part, medium-viscosity UV/visible-light-curing acrylated urethane adhesive for flexible material bonding in medical-device assembly. The transparent, fluorescent material bonds plasticized PVC, thermoplastic elastomers, thermoset rubbers, and compatible rigid plastics. On glass, fixture is achieved in 5 seconds or less with 405 nm LED light at 10 mW/cm^2. After 10 seconds at 1 W/cm^2 and 405 nm, typical cured properties include 233% elongation and 22.1 N/mm^2 tensile strength, combining flexible mechanical response with fast light processing. Cure and bond results depend on light dose, substrate, geometry, and preparation.

Key features

  • Medium-viscosity flexible bonding: Cone-and-plate viscosity is 300 to 800 mPa s (cP) at 25 deg C and a shear rate of 180 s^-1.
  • Fast 405 nm LED fixture: Fixture is 5 seconds or less on glass at 10 mW/cm^2 measured at 405 nm.
  • Cured flexibility: Typical elongation at break is 233% after 10 seconds at 1 W/cm^2 and 405 nm.

Applications

Bonding flexible materials including plasticized PVC, TPE and thermoset rubbers in medical-device assemblies.

Product Family

LOCTITE AA 3953

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Transparent, colorless to straw colored liquid
Chemistry TypeChemistry Type
Acrylated urethane
Specific GravitySpecific Gravity
~1.07
Physical Properties
ViscosityViscosity
300 to 800 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
13.5 °C
Mechanical Properties
ElongationElongation
233 %
Chemical Properties
Water AbsorptionWater Absorption
8.4 %
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceTransparent, colorless to straw liquidUncured
UV fluorescencePositiveUnder UV light
Specific gravityApprox. 1.0725 deg C
Cone and plate viscosity300 to 800mPa s (cP)25 deg C; shear rate 180 s^-1
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shore hardness56Durometer DISO 868; 1 W/cm^2 at 405 nm for 10 s
Elongation at break233%ISO 527-3; 1 W/cm^2 at 405 nm for 10 s
Tensile strength22.1N/mm^2ISO 527-3; 1 W/cm^2 at 405 nm for 10 s
PC-to-PVC block shear5.0N/mm^2ISO 13445; 1 W/cm^2 at 405 nm for 10 s
Grit-blasted PC-to-PC block shear22.5N/mm^2ISO 13445; 1 W/cm^2 at 405 nm for 10 s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers