LOCTITE EA 9005CL

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9005CL

Main features

  • Ultra Fast Cure
  • Flexible Cured Epoxy
  • Optically Clear Performance

Product Description

LOCTITE EA 9005CL is a two-component, room-temperature curing epoxy potting compound formulated for applications requiring rapid processing and flexibility. This ultra-fast curing epoxy is supplied in a 1:1 mix ratio and develops handling strength in less than 7 minutes on common substrates. Its clear appearance, high light transmission, and flexible cured profile make it suitable for overmolding and potting applications, particularly in cable assemblies where high throughput and fast fixture times are important. The cured material provides elongation of approximately 49.3%, Shore A hardness of 84, and dielectric breakdown strength of 18.5 kV/mm.

Key features

  • Ultra-fast cure: Develops fixture strength in less than 7 minutes on common substrates to support high-throughput manufacturing.
  • Flexible cured epoxy: Delivers approximately 49.3% elongation at break for applications where flexibility is beneficial.
  • Optically clear performance: Provides greater than 91% light transmission at 550 nm after cure.

Applications / Suitable for

  • Cable overmolding applications
  • Potting and encapsulation
  • Electrical and electronic component protection
  • Fast-cycle production environments
Product Family

LOCTITE EA 9005CL

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two Part (Resin | Hardener)
Specific GravitySpecific Gravity
1.16
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
7 °C
Mechanical Properties
ElongationElongation
49.3 %
Electrical Properties
Dielectric StrengthDielectric Strength
18.5 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for supplied components and mixed material.

Property Value Unit Method / condition
Mix Ratio 1:1 Volume Resin : Hardener
Gel Time 7 to 12 minutes 22°C
Mixed Specific Gravity 1.16 - 25°C
Mixed Viscosity 8,000 to 15,000 mPa·s Hardener, CP25-2, 20 s⁻¹
Technical properties

After-processing / final-state properties

Typical cured-material properties after 5 days at 22°C unless otherwise noted.

Property Value Unit Method / condition
Shore Hardness 84 Shore A ISO 868
Elongation at Break 49.3 % ISO 527-3
Tensile Strength 1.6 N/mm² ISO 527-3
Dielectric Breakdown Strength 18.5 kV/mm IEC 60243-1
Light Transmission >91.8 % 550 nm, ASTM D1003

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers