Loctite EA 9377

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 937.7

Main features

  • 2,000-Cycle Thermal-Crack Resistance
  • 124 MPa Compressive Strength
  • 5 mil Low-Slump Moldable Shim

Product Description

LOCTITE® EA 9377 AERO is a two-component epoxy paste adhesive formulated as a moldable plastic shim for aerospace assemblies. The low-slump material can produce shim sections as thin as 5 mil and cures at room temperature, with accelerated thermal curing available for small mixed masses. Its cured properties include high compressive strength and resistance to visible microcracking through a documented 2,000-cycle thermal-cycling sequence. The adhesive develops handling strength after 24 hours at 77°F (25°C) and may be fully cured in 5–7 days at the same temperature or in 1 hour at 180°F (82°C). It is qualified to BMS 8-338.

Key features

  • Thermal-cycling resistance: Little or no cracking visible to the unaided eye after a documented sequence totaling 2,000 thermal cycles.
  • High compressive performance: Typical compressive strength at 2% strain is 18.0 ksi (124 MPa) at 77°F (25°C).
  • Controlled shim application: Low-slump consistency supports moldable plastic shim sections down to a minimum thickness of 5 mil.

Applications / Suitable for

  • Moldable plastic shim applications in aerospace assemblies
  • Thin shim sections requiring a minimum thickness down to 5 mil
  • Assemblies exposed to repeated thermal cycling
Product Family

LOCTITE EA 9377

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity (Part A)Viscosity (Part A)
220,000 mPa.s
Viscosity (Part B)Viscosity (Part B)
89,000 mPa.s
General Properties
Mix RatioMix Ratio
100:19

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-material, storage, working-time, and cure information for LOCTITE® EA 9377 AERO.

Property Value Unit Method / condition
Product type Two-component epoxy paste adhesive and moldable plastic shim — As supplied
Color Part A: Gray; Part B: Black; Mixed: Dark gray — Visual
Viscosity, Part A 2,200 Poise 77°F; Brookfield HBT, spindle 7 at 20 rpm
Viscosity, Part B 890 Poise 77°F; Brookfield HBT, spindle 6 at 20 rpm
Viscosity, Part A 220 Pa·s 25°C; Brookfield HBT, spindle 6 at 2.1 rad/s
Viscosity, Part B 89 Pa·s 25°C; Brookfield HBT, spindle 5 at 2.1 rad/s
Density Part A: 1.55; Part B: 1.08; Mixed: 1.44 g/mL As supplied and mixed states
Mix ratio 100:19 Parts by weight Part A:Part B; volume measurement is not recommended for structural applications
Pot life 60 minutes 100 g mass at 77°F (25°C); ASTM D2471, water bath
Handling strength time 24 hours At 77°F (25°C); full bond strength has not yet been attained
Room-temperature cure 5–7 days At 77°F (25°C)
Example accelerated cure 1 hour at 180°F (82°C) — Provides complete cure; accelerated cures up to 200°F (93°C) are stated for small masses only
Minimum shim thickness capability 5 mil Minimum stated shim thickness
Shelf life, Part A 6 months; 3 months — 6 months at <40°F (4°C); 3 months at <77°F (25°C)
Shelf life, Part B 12 months — At either <40°F (4°C) or <77°F (25°C)
Available dispensing format 6 oz barrier-type Semkits® — Documented packaging option for dispensing
Technical properties

After-processing / final-state properties

Typical cured mechanical and thermal-cycling performance. Values depend on the stated cure, substrate, specimen, test method, and test temperature.

Property Value Unit Method / condition
Tensile lap shear strength 2,300 psi (15.8 MPa) ASTM D1002; tested at −67°F (−55°C); 2024-T3 bare aluminum; cured 5 days at 77°F (25°C)
Tensile lap shear strength 2,300 psi (15.8 MPa) ASTM D1002; tested at 77°F (25°C); 2024-T3 bare aluminum; cured 5 days at 77°F (25°C)
Tensile lap shear strength 2,100 psi (14.5 MPa) ASTM D1002; tested at 190°F (88°C); 2024-T3 bare aluminum; cured 5 days at 77°F (25°C)
Shore D hardness 85 Shore D After 72-hour cure at 77°F (25°C)
Compressive modulus 904 ksi (6,234 MPa) ASTM D695; tested at 77°F (25°C); cylindrical specimen 0.5 in (12.7 mm) diameter × 1 in (25.4 mm)
Compressive strength at 2% strain 18.0 ksi (124 MPa) ASTM D695; tested at 77°F (25°C); cylindrical specimen 0.5 in (12.7 mm) diameter × 1 in (25.4 mm)
Compressive modulus 400 ksi (2,759 MPa) ASTM D695; tested at 190°F (88°C); cylindrical specimen 0.5 in (12.7 mm) diameter × 1 in (25.4 mm)
Compressive strength at 2% strain 8.0 ksi (55 MPa) ASTM D695; tested at 190°F (88°C); cylindrical specimen 0.5 in (12.7 mm) diameter × 1 in (25.4 mm)
Thermal-cycling performance Little or no cracking visible to the unaided eye — 12 hours at 120°F (49°C) condensing humidity; 1 hour at −67°F (−55°C); 400 cycles between −67°F (−55°C) and 160°F (71°C) at 36 minutes per cycle; sequence repeated five times for 2,000 cycles
Qualification BMS 8-338 — Qualification stated in the July 2013 Technical Process Bulletin

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers