Main features

  • Nickel-Based High-Temperature Anti-Seize
  • Galling and Corrosion Protection
  • Threaded and Press-Fit Assembly Use

Product Description

LOCTITE LB 771 is a non-curing nickel-based anti-seize lubricant paste for threaded and press-fit assemblies exposed to high temperature and heavy pressure. The thick metallic-silver paste contains mineral oil, nickel, and graphite and remains a lubricating anti-seize layer rather than forming a cured film. Its operating range is -54 to 1315 deg C, with a typical viscosity range of 650,000 to 1,050,000 mPa s at 25 deg C. It reduces friction during tight assembly of stainless-steel threads and press fits and resists galling, corrosion, and wear while allowing easier disassembly after hot or corrosive exposure. It is not intended as a high-speed load-carrying lubricant for ball or roller bearings.

Key features

  • Nickel/Graphite Anti-Seize: Mineral-oil paste containing nickel and graphite for heavy-duty anti-seize lubrication.
  • High-Temperature Operating Range: Used across an operating range of -54 to 1315 deg C.
  • Stainless-Steel Assembly Protection: Reduces friction and galling during assembly of stainless-steel threads and press-fit components.

Applications

Stainless-steel threaded and press-fit assemblies, chemical-plant bolts, pump housings, pipe flanges, drop-forge dies, hammers, and conveyor chains.

Product Family

LOCTITE LB 771

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Thick metallic, silver paste, without separation
Chemistry TypeChemistry Type
Mineral oil, nickel, graphite
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
650,000 to 1,050,00 mPa.s
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Specific gravity1.1-Typical; 25 deg C
Viscosity650,000 to 1,050,000mPa sLMS range; Brookfield RVT, 25 deg C, spindle TE, 2.5 rpm
Operating range-54 to 1315deg CTypical application range
AppearanceThick metallic silver paste-LMS appearance; without separation

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers