LOCTITE LB 8044
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- 398 deg C Anti-Seize Range
- Aluminum Hardware Anti-Seize
- 0.15 Tested Torque Coefficient
Product Description
LOCTITE LB 8044 combines zinc dust and petrolatum in a non-curing zinc-based anti-seize paste. It is used on threaded and unthreaded metal joints, with particular application to aluminum and aluminum-alloy hardware, and also provides corrosion protection for aluminum and ferrous components. Typical applications include bolts, screws, studs, pipe joints, nuts, and plugs. Typical operating range for applications is -29 to 398 deg C. On 12.7 mm grade 8 steel bolts with grade 5 nuts, a torque coefficient of 0.15 was measured, compared with 0.27 for solvent-cleaned, unlubricated hardware.
Key features
- Zinc-Based Anti-Seize: Smooth paste formulated from zinc dust and petrolatum.
- Aluminum Joint Application: Used on aluminum and aluminum-alloy bolts, screws, studs, pipe joints, nuts, and plugs.
- 0.15 Torque Coefficient: Measured on 12.7 mm grade 8 steel bolts with grade 5 nuts.
Applications
Threaded and unthreaded metal assemblies, particularly aluminum and aluminum-alloy bolts, screws, studs, pipe joints, nuts, and plugs.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Dull silver smooth paste | As supplied | |
| Specific gravity | 1.36 | 25 deg C | |
| Weight per gallon | 10.8 to 11.8 | lb/gal | Typical |
| Penetration | 160 to 280 | 1/10 mm | ISO 2137 |