LOCTITE UR 3371

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

LOCTITE UR3371

Main features

  • 40-Minute Skin-Over Time
  • -30 to 80 deg C Service Range
  • More Than 300% Cured Elongation

Product Description

LOCTITE UR 3371 is a one-part polyurethane adhesive/sealant supplied as a paste and cured by atmospheric moisture. It is available in gray, black, and white and is applied from 5 to 38 deg C. Typical curing data at 23 deg C and 50% RH include a 40-minute skin-over time, 50 to 70 minute tack-free time, and 3 mm cure rate after 24 hours. After 7 days under the same conditions, typical cured properties include Shore A hardness 50 and elongation greater than 300%.

Key features

  • Surface Skin Formation: Typical skin-over time is 40 minutes at 23 deg C and 50% RH.
  • Temperature Capability: In-service temperature range is -30 to 80 deg C.
  • Cured Flexibility: Typical elongation at break is greater than 300% after seven days at 23 deg C and 50% RH.

Applications

Sealing and bonding side panels; elastic interior and exterior seams and joints in specialty vehicles and caravans.

Product Family

LOCTITE UR 3371

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.08
Mechanical Properties
ElongationElongation
300 %

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
AppearanceGray, black, whiteAs supplied
FormPasteAs supplied
Specific gravity1.0823 deg C
Extrusion rate300g/min60 seconds at 23 deg C; 0.6 MPa pressure
Technical properties

Final-state properties

Typical cured properties after 7 days at 23 deg C and 50% RH.

PropertyValueUnitMethod / condition
Shore hardness50Shore AASTM D 412; cured 7 days at 23 deg C, 50% RH
Elongation at breakGreater than 300%ASTM D 412; cured 7 days at 23 deg C, 50% RH
Tensile strengthGreater than 2.5N/mm2ASTM 412C; cured 7 days at 23 deg C, 50% RH

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers