PERMABOND UV6231

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

PERMABOND UV6231

Main features

  • Optically Clear Glass and Crystal Bonding
  • 2-Second LED Fixture
  • Humidity-Resistant High-Elongation UV Bond

Product Description

Permabond UV6231 is a single-part optically clear UV-curable adhesive for glass, crystal and glass-to-metal assemblies. It cures across 365-400 nm and reaches typical fixture in 2 seconds under a 100 mW/cm2 LED source; cure time varies with lamp output, distance and substrate transmission. After cure, typical steel-to-glass tensile strength is 10 N/mm2 and elongation exceeds 120%. After 500 hours at 70 deg C and 90% relative humidity, steel-to-glass tensile strength is 6-7 N/mm2. The adhesive is used in bathroom-type and outdoor assemblies requiring moisture, humidity and weathering resistance.

Key features

  • Optically clear glass and crystal bonding: The cured adhesive remains clear and resists yellowing for glass and crystal assemblies.
  • 2-second LED fixture: Typical fixture is 2 seconds under a 100 mW/cm2 LED source; actual cure time depends on the UV setup and substrate transmission.
  • 500-hour humidity-conditioned strength: Steel-to-glass tensile strength is 6-7 N/mm2 after 500 hours at 70 deg C and 90% relative humidity.

Applications

Glass and crystal bonding; glass-to-metal bonding; bathroom-type assemblies; outdoor assemblies.

Product Family

PERMABOND UV6231

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless, clear
Chemistry TypeChemistry Type
Methacrylate ester
Refractive indexRefractive index
1.490
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
5,000-8,000 mPa.s
Mechanical Properties
ElongationElongation
120 %
Electrical Properties
Dielectric StrengthDielectric Strength
12 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionMethacrylate ester-Uncured adhesive
AppearanceColorless, clear-Uncured adhesive
Viscosity at 20 rpm5,000-8,000cP25 deg C
Specific gravity1.1-Uncured adhesive
Cure wavelength365-400nmUV cure
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Steel-to-glass tensile strength10N/mm2Typical cured joint; ASTM D-2095-69
Elongation>120%Typical cured adhesive; ISO 37
Hardness45-50Shore DTypical cured adhesive; ISO 868
Humidity-conditioned tensile strength6-7N/mm2Steel to glass; 500 h at 70 deg C / 90% RH; ASTM D-2095-69

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers