PERMABOND UV632

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

PERMABOND UV632

Main features

  • Long-Wavelength UV-Stabilized Plastic Bonding
  • Low-Viscosity 200-400 cP Application
  • 4-Second Acrylic Fixture

Product Description

Permabond UV632 is a low-viscosity UV-curable adhesive for acrylic and other selected plastics, including many UV-stabilized plastic assemblies. Its long-wavelength photoinitiator cures across 365-420 nm, and viscosity is 200-400 cP at 25 deg C. Typical fixture on acrylic is 4 seconds under a 100 mW/cm2 LED source; actual cure time depends on lamp output, distance and substrate transmission. After cure, overlap shear exceeds 7 N/mm2 on polycarbonate and 4 N/mm2 on PET, with substrate failure in both tests. UV632 can also bond glass and metals when the bondline is accessible to UV light.

Key features

  • 365-420 nm plastic-bonding cure range: The long-wavelength cure range allows bonding through many UV-stabilized plastics.
  • 200-400 cP low viscosity: Low viscosity at 25 deg C supports application to close-fitting plastic assemblies.
  • 4-second acrylic fixture: Typical fixture is 4 seconds on acrylic under a 100 mW/cm2 LED source.

Applications

Bonding acrylic and other selected plastics; bonding UV-stabilized plastic assemblies; glass and metal bonding.

Product Family

PERMABOND UV632

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless, clear
Chemistry TypeChemistry Type
Urethane methacrylate
Refractive indexRefractive index
1.490
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
200-400 mPa.s
Mechanical Properties
ElongationElongation
70 %
Electrical Properties
Dielectric StrengthDielectric Strength
25 - 30 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionUrethane methacrylate-Uncured adhesive
AppearanceColorless, clear-Uncured adhesive
Viscosity at 20 rpm200-400cP25 deg C
Specific gravity1.1-Uncured adhesive
Cure wavelength365-420nmUV cure
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Overlap shear strength>7N/mm2Typical cured joint; polycarbonate; ISO 4587; substrate failure
Overlap shear strength>3N/mm2Typical cured joint; acrylic; ISO 4587
Overlap shear strength>4N/mm2Typical cured joint; PET; ISO 4587; substrate failure
Tensile strength13N/mm2Typical cured adhesive; ISO 37
Elongation at break>70%Typical cured adhesive; ISO 37

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers