PERMATEX 133-K
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- Aluminum-Copper-Graphite Anti-Seize Blend
- Service to 870 deg C
- Meets MIL-A-907E Requirements
Product Description
Permatex Anti-Seize Lubricant, 8 oz is a heavy-duty anti-seize lubricant containing aluminum, copper and graphite lubricating solids for high-temperature threaded and slow-moving assemblies. The metallic paste has a typical viscosity of 100,000-200,000 cP and a specific gravity of 1.13. Its stated service range extends from -51 to 870 deg C. The lubricant is used to reduce galling, seizing and wear under heavy contact pressure while supporting later disassembly of heat-exposed or corrosive assemblies. The product meets or exceeds the requirements of MIL-A-907E and is not intended for wheel lug nut or stud applications.
Key features
- Aluminum, copper and graphite anti-seize: The lubricating-solid blend is formulated for threaded and slow-moving assemblies exposed to heat and pressure.
- Service range to 870 deg C: The stated temperature range is -51 to 870 deg C.
- MIL-A-907E requirement: The product meets or exceeds the requirements of Military Specification MIL-A-907E.
Applications
Spark-plug threads; exhaust-manifold and engine bolts; brake anchor pins; U-bolts and spring bolts; hinges, gears, chains, sprockets and rollers; boiler and oven parts.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical type | Grease | - | As supplied |
| Lubricating solids | Aluminum, copper and graphite | - | As supplied |
| Specific gravity | 1.13 | - | As supplied |
| Viscosity | 100,000-200,000 | cP | As supplied |
| Flash point | >350 | deg F | As supplied |