PLEXUS MA1025

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

PLEXUS MA1025

Main features

  • 20-25 Minute Work, 40-45 Minute Fixture
  • 2-25 mm Structural Gap Filling
  • 90-110% Cured Strain

Product Description

Plexus MA1025 is a two-part 10:1 methacrylate structural adhesive with low cure shrinkage and low odor for thermoplastic, metal and composite assemblies. At 23 deg C, working time is 20-25 minutes and fixture time is 40-45 minutes. The non-sagging adhesive fills bond gaps from 2 to 25 mm and requires little surface preparation for supported substrates. After cure, typical tensile strength is 9.7-12.4 MPa, tensile modulus is 414-552 MPa and strain to failure is 90-110%. Typical lap-shear cohesive strength is 8.3-13.8 MPa to ASTM D1002.

Key features

  • 20-25 minute working time: Working time is 20-25 minutes at 23 deg C, with fixture time in 40-45 minutes.
  • 2-25 mm gap filling: The non-sagging 10:1 adhesive is specified for bond gaps from 2 to 25 mm.
  • 90-110% strain to failure: Typical cured strain to failure is 90-110%, with tensile strength of 9.7-12.4 MPa.

Applications

Structural bonding of thermoplastics, metals and composites; bonding stringers and liners in fiberglass boats; other supported marine structural assemblies.

Product Family

PLEXUS MA1025

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-White/Blue
Density (g)Density (g)
0.97/1.07 g/cm3
Mix RatioMix Ratio
10:1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
180,000–220,000 mPa.s
Viscosity (Part B)Viscosity (Part B)
35,000–70,000 mPa.s
Mechanical Properties
ElongationElongation
90 - 110 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part A viscosity180,000-220,000cPUncured adhesive
Part B viscosity35,000-70,000cPUncured activator
Part A density0.97g/ccUncured adhesive
Part B density1.07g/ccUncured activator
Mix ratio by volume10:1-Part A : Part B
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile strength9.7-12.4MPaTypical cured adhesive; ASTM D638
Tensile modulus414-552MPaTypical cured adhesive; ASTM D638
Strain to failure90-110%Typical cured adhesive; ASTM D638
Lap-shear cohesive strength8.3-13.8MPaTypical cured joint; ASTM D1002

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers