PLEXUS MA2015

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

PLEXUS MA2015

Main features

  • 15-18 Minute Work Time
  • 0.75-38 mm Gap Filling
  • 19.8-24.8 MPa Tensile Strength

Product Description

Plexus MA2015 White is a two-part 10:1 methacrylate structural adhesive for thermoplastic, metal and composite assemblies with UV- and yellowing-resistant white appearance. At 23.9 deg C, typical work time is 15-18 minutes. The adhesive fills gaps from 0.75 to 38 mm, with final gap capability dependent on laminate thickness and composition. After cure, typical tensile strength is 19.8-24.8 MPa, tensile modulus is 985-1,103 MPa and elongation at break is 21-54%. Typical aluminum lap-shear strength is 17.3 MPa.

Key features

  • 15-18 minute work time: Typical work time is 15-18 minutes at 23.9 deg C.
  • Gap filling from 0.75 to 38 mm: The adhesive fills gaps from 0.75 to 38 mm, subject to laminate thickness and composition.
  • 19.8-24.8 MPa tensile strength: Typical cured tensile strength is 19.8-24.8 MPa with 21-54% elongation at break.

Applications

Structural bonding of thermoplastics, metals and composites; composite bonding in marine and transportation assemblies.

Product Family

PLEXUS MA2015

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-White/White
Density (g)Density (g)
0.99/1.47 g/cm3
Mix RatioMix Ratio
10:1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
180 - 220 mPa.s
Viscosity (Part B)Viscosity (Part B)
35 - 70 mPa.s
Mechanical Properties
ElongationElongation
21 - 54 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part A viscosity180,000-220,000cPUncured adhesive
Part B viscosity35,000-70,000cPUncured activator
Part A density0.99g/mlUncured adhesive
Part B density1.47g/mlUncured activator
Mix ratio by volume10:1-Part A : Part B
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile strength19.8-24.8MPaTypical cured adhesive; ASTM D638 / ISO 527
Tensile modulus985-1,103MPaTypical cured adhesive; ASTM D638 / ISO 527
Elongation at break21-54%Typical cured adhesive; ASTM D638 / ISO 527
Lap-shear strength17.3MPaTypical cured joint; aluminum; ASTM D1002

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers